2379 Steel, D2, SKD11, XW41, XW42 Tool Steel  Tool Steel


We are the Leading Supplier of XW41 Tool Steel. 
2379 / SKD11 Steel is Chrome steel 12% with very high resistance against abrasive and adhesive wear due to a high volume of hard carbides in the steel matrix, good toughness, very good dimensional stability, high compressive strength, very good base material for PVD/CVD coating as well as nitriding due to its secondary hardening properties.

We supply and export to Singapore , Indonesia , Brunei and other ASEAN Countries.  
Our specialty is to provide wide range of stainless steel
 with no minimum order (MOQ).

E Steel supply Tool Steel 2379 (SKD11) Round Bars/ Rods/ Shafts , D2 (XW41) Plates.  




2379 Steel Suppliers - XW41, XW42, SKD11, D2 Tool Steel (X153CrMoV12) 

XW41 Tool Steel is a Chrome steel 12%, very high resistance against abrasive and adhesive wear due to a high volume of hard carbides in the steel matrix, good toughness, very good dimensional stability, high compressive strength, very good base material for PVD/CVD coating as well as nitriding due to its secondary hardening properties. Similar to SKD11 / 2379

Applications of XW41 / XW42 Steel 

Tool Steel 2379 can be used for :

Cutting, punching, stamping tools, shear blades, thread rolling dies, cold extrusion dies, drawing and bending tools, flanging and straightening rolls, fine cutting tools, deep drawing tools, plastic moulds for abrasive polymers.


Chemical Composition of D2 Steel 

 

Chemical Composition %
Carbon 1.55
Chromium 12.00
Molybdenum 0.80
Vanadium 0.90

D2 Steel is equivalent to 

Country USA German Japan
Standard ASTM A681 DIN EN ISO 4957 JIS G4404
Grades D2 1.2379/X153CrMo12 SKD11

Mechanical Properties of 2379 Steel 

Mechanical Properties Metric Imperial
Hardness, Knoop (converted from Rockwell C hardness) 769 769
Hardness, Rockwell C 62 62
Hardness, Vickers 748 748
Izod impact unnotched 77.0 J 56.8 ft-lb
Poisson’s ratio 0.27-0.30 0.27-0.30
Elastic modulus 190-210 GPa 27557-30457 ksi

Heat Treatment of D2 Steel 

Soft Annealing

Temperature Cooling Hardness
820 – 850oC furnace max 255 HB

Stress Relief Annealing

Temperature Cooling
600 – 650oC Furnace

Hardening

Temperature Cooling Tempering
1020 – 1030oC oil, pressure (N2)
air or hot bath
500 – 550oC
see tempering diagram
usually < 300°C
1040 – 1080oC oil, pressure (N2)
air or hot bath
500 – 550oC
see tempering diagram
usually 500°C


Our Sales & Supplier Network

Australia, Pakistan,  Malaysia, Singapore, Taiwan, China,Vietnam, Belgium, Japan, South Korea, Philippines, France, United Kingdom, Indonesia, Thailand, Hong Kong, China, Sweden, United States, Dubai, Finland, Brunei,Germany.]



OUR MOTTO : ” WHY BUY A FULL BAR OR SHEET WHEN YOU JUST NEED A SMALL VOLUME?




Please leave your enquiry here, we will reply as soon as possible.
Name*  
Company Name  
Product Interested  
Quantity  
Email*  
Contact No.*  
Attachment  
*only support gif, jpeg, jpg, png, pdf
Messages*  

Switch to Mobile Version